Dow Corning 9040 Silicone Elastomer Blend

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 9040 Silicone Elastomer Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, haircare, color cosmetics, suncare, antiperspirants and deodorants, and wouldcare applications.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc

@Temperature 25.0 °C
0.960 g/cc

@Temperature 77.0 °F
Viscosity Measure 250000 - 580000 cSt
250000 - 580000 cSt
Kinetic/Kinematic
Descriptive Properties Value Comments
Cyclotetrasiloxane Content (%) <1
Nonvolatile Content (%) 12-12.75