Dow Corning HV 1650/50 SILICONE RUBBER

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning HV 1650/50 SILICONE RUBBER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50 Shore A hardness high consistency silicone rubber with excellent tracking and erosion resistance and low modulusInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc

@Temperature 25.0 °C
1.50 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Ultimate 5.00 MPa
725 psi
Elongation at Break 450 %
450 %
Tear Strength 17.0 kN/m
97.0 pli
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+14 ohm-cm
1.60e+14 ohm-cm
Dielectric Constant 3.51

@Frequency 100 Hz
3.51

@Frequency 100 Hz
Dielectric Strength 16.4 kV/mm
416 kV/in
Dissipation Factor 0.034

@Frequency 100 Hz
0.034

@Frequency 100 Hz
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color grey
Hydrophobic yes