Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning JCR 6101

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning JCR 6101.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part, translucent, medium modulus LED encapsulant with very long working time.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity 5900 cP
5900 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
Tensile Strength, Ultimate 1.700 MPa
246.6 psi
Elongation at Break 170 %
170 %
Optical Properties Metric English Comments
Refractive Index 1.398
1.398
1.407
1.407
1.397

@Wavelength 1554 nm
1.397

@Wavelength 1554 nm
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 70.0 °C
1.00 hour

@Temperature 158 °F
120 min

@Temperature 150 °C
2.00 hour

@Temperature 302 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Appearance translucent
Users viewing this material also viewed the following: