Dow Corning JCR 6115

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Encapsulation Grade
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning JCR 6115.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, fast cure, low modulus LED encapsulant with low viscosity and very long working time.Information provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 13
13
Tensile Strength, Ultimate 0.400 MPa
58.0 psi
Elongation at Break 130 %
130 %
Optical Properties Metric English Comments
Refractive Index 1.396
1.396
1.404
1.404
1.395

@Wavelength 1554 nm
1.395

@Wavelength 1554 nm
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 175 °C
0.0833 hour

@Temperature 347 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Mix Ratio (X:1) 100
Base to Catalyst ETN