Silicone grease with wide service temperature rangeInformation provided by Dow Corning
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 325
325
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 280 °C
536 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Dropping Point >= 210 °C
>= 410 °F
Descriptive Properties Value Comments
Color white
Thickening System lithium