Dow Corning MOLYKOTE® G-1001

Category Fluid , Lubricant
Manufacturer Dow Corning
Trade Name MOLYKOTE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning MOLYKOTE® G-1001.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multipurpose bearing grease based on a blend of mineral and synthetic oilsInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc

@Temperature 25.0 °C
0.910 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 179.9 kg
396.7 lb (mass)
Penetration P(60), 1/10 mm 250
250
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Dropping Point >= 260 °C
>= 500 °F
Descriptive Properties Value Comments
Color light brown
NLGI Number 3
Thickening System lithium complex
Water Resistant yes