Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning MOLYKOTE® LONGTERM 2 PLUS

Category Fluid , Lubricant
Manufacturer Dow Corning
Trade Name MOLYKOTE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning MOLYKOTE® LONGTERM 2 PLUS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Performance Mineral Oil GreaseInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc

@Temperature 25.0 °C
0.900 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 387.4 kg
854.2 lb (mass)
Penetration P(60), 1/10 mm 265 - 295
265 - 295
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -25.0 °C
-13.0 °F
Dropping Point >= 175 °C
>= 347 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Descriptive Properties Value Comments
Color black
NLGI Number 2
Users viewing this material also viewed the following: