Dow Corning Q2-1607 EMULSION

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Q2-1607 EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
36% emulsion that is used both for sofening and providing water repellency to textile substrates. Contains a silicone polymer that has been slightly crosslinked to give it a differential 'hand' compared to traditional softeners.Information provided by Dow Corning
Physical Properties Metric English Comments
pH 5.0 - 7.0
5.0 - 7.0
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Active Content (%) 36
Cationic yes
Color white