Material Notes:
A heat-cured elastomer for use by customers fabricating medical devices, including those intended for implantation in humans for less than 30 days and non-implant applications. Dow Corning® S40 Liquid Silicone Rubber is a two-part platinumcatalyzed silicone elastomers specifically designed for liquid injection molding or supported extrusion. The elastomer is supplied as a two-part kit (Part A and Part B), equal portions (by weight) of which must be thoroughly blended together prior to use. The elastomer is thermally cured via an addition-cure (platinum catalyzed) reaction. When blended and cured as indicated the resulting elastomer consists of crosslinked dimethyl and methyl-vinyl siloxane copolymers and reinforcing silica.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength, Ultimate 8.62 MPa
1250 psi
Elongation at Break 684 %
684 %
Tear Strength 31.2 kN/m
178 pli
Compression Set 18 %
18 %