Dow Corning SILASTIC® LS 4-9080 FLUOROSILICONE RUBBER

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® LS 4-9080 FLUOROSILICONE RUBBER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc

@Temperature 25.0 °C
1.55 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
Tensile Strength, Ultimate 7.52 MPa
1090 psi
Tensile Strength, Yield 5.63 MPa
816 psi
at 150% Elongation, maximum
Elongation at Break 159 %
159 %
Tear Strength 20.0 kN/m
114 pli
Compression Set 11 %
11 %
Thermal Properties Metric English Comments
Shrinkage 3.3 %
3.3 %
after 7 days
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Color off-white