Dow Corning SILASTIC® LSR 9682-50 PARTS A&B

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® LSR 9682-50 PARTS A&B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50 Durometer, 2-part, 1 to 1 mix, clear Liquid Silicone RubberInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc

@Temperature 25.0 °C
1.14 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Ultimate 9.51 MPa
1380 psi
Tensile Strength, Yield 1.65 MPa
240 psi
at 150% Elongation, maximum
Elongation at Break 620 %
620 %
Tear Strength 48.2 kN/m
275 pli
Compression Set 20.9 %
20.9 %
Processing Properties Metric English Comments
Pot Life 1440 min
1440 min
Descriptive Properties Value Comments
Appearance translucent
Color light blue
Mix Ratio (X:1) 100