Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SILASTIC® Q7-4765 BIOMEDICAL GRADE ETR ELASTOMER, KIT

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® Q7-4765 BIOMEDICAL GRADE ETR ELASTOMER, KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, platinum-catalyzed (1:1 by weight), enhanced tear-resistant silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices.Information provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Ultimate 8.00 MPa
1160 psi
Elongation at Break 900 %
900 %
Tear Strength 45.6 kN/m
260 pli
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved