Dow Corning SM 8715 EX

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SM 8715 EX.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A reactive epoxyfunctional silicone emulsion; imparts very good water repellency, very good stability, high whiteness retention and improves fabric physical properties.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc

@Temperature 25.0 °C
1.00 g/cc

@Temperature 77.0 °F
Solids Content 40 %
40 %
pH 7.0
7.0
Processing Properties Metric English Comments
Shelf Life 9.00 Month
9.00 Month
Descriptive Properties Value Comments
Color Milky White
Hydrophobic Yes
Non-Ionic Yes