Material Notes:
C4-2109 is a 10% active solids solution of a silicate based compound. This product is recommended for use as a release modifier for Syl-Off® brand solvent based, condensation curing, systems.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc

@Temperature 25.0 °C
0.900 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 1.0 cSt

@Temperature 25.0 °C
1.0 cSt

@Temperature 77.0 °F
Storage Temperature <= 50.0 °C
<= 122 °F
Thermal Properties Metric English Comments
Flash Point 27.0 °C
80.6 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 10
Appearance liquid
Color watery white
Solvent Xylene