Dow Corning SYL-OFF® SL 7028 CROSSLINKER

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® SL 7028 CROSSLINKER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solvent-free, but suitable for both solvent and solventless coatingInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.997 g/cc

@Temperature 25.0 °C
0.997 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Kinematic Viscosity 20 cSt
20 cSt
Thermal Properties Metric English Comments
Flash Point 74.0 °C
165 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance colorless liquid
Solvent solventless