Material Notes:
Is chemically equivalent to DOW CORNING® 536 FLUID. 100 % active, amino methoxy functional polydimethylsiloxane.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.985 g/cc

@Temperature 25.0 °C
0.985 g/cc

@Temperature 77.0 °F
Viscosity Measure 40 cSt
40 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point 15.6 °C
60.1 °F
Closed cup
Optical Properties Metric English Comments
Refractive Index 1.408
1.408
Descriptive Properties Value Comments
Active Content (%) 100
Color Clear colorless liquid