Dow Corning XIAMETER® PMCPPMX-0344 Cyclosiloxane Blend

Category Fluid , Polymer , Thermoplastic , Siloxane
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPPMX-0344 Cyclosiloxane Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 344 FLUID. A volatile methylsiloxane fluid, clear, odorless, VOC-exempt, low toxicity, low surface tension, evaporates completely at room temperatureInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc

@Temperature 25.0 °C
0.950 g/cc

@Temperature 77.0 °F
Viscosity Measure 2.5 cSt
2.5 cSt
Kinetic/Kinematic
Surface Tension 19 dynes/cm
19 dynes/cm
Thermal Properties Metric English Comments
Melting Point 15.0 °C
59.0 °F
Boiling Point 177 °C
351 °F
Flash Point 52.0 °C
126 °F
Closed Cup
Processing Properties Metric English Comments
Shelf Life 30.0 Month
30.0 Month