Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning XIAMETER® PMCPPMX-200 20Cs Silicone Fluid

Category Fluid
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPPMX-200 20Cs Silicone Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 200 FLUID 20CS. 100% active, 20 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.949 g/cc

@Temperature 25.0 °C
0.949 g/cc

@Temperature 77.0 °F
Viscosity Measure 20 cSt
20 cSt
Kinetic/Kinematic
Surface Tension 20.6 dynes/cm
20.6 dynes/cm
Thermal Properties Metric English Comments
Thermal Conductivity 0.142 W/m-K
0.985 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Pour Point -84.0 °C
-119 °F
Flash Point >= 204 °C
>= 399 °F
Open Cup
246 °C
475 °F
Closed Cup
Optical Properties Metric English Comments
Refractive Index 1.40
1.40
Descriptive Properties Value Comments
Hydrophobic Yes
Users viewing this material also viewed the following: