Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
Kinematic Viscosity 0.46 cSt
0.46 cSt
Vapor Pressure 0.1700 bar

@Temperature 25.0 °C
127.5 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Melting Point -76.0 °C
-105 °F
Boiling Point 66.0 °C
151 °F
Flash Point 3.00 °C
37.4 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Descriptive Properties Value Comments
Appearance colorless
Color light straw
Hydrophobic yes