Material Notes:
Aminoethylaminopropyltrimethoxysilane - H2NC2H4NHC3H6-Si(OCH3)3 Coupling agent for many thermoset and thermoplastic resins with glass or mineral fillers.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Kinematic Viscosity 5.0 cSt
5.0 cSt
Molecular Weight 222 g/mol
222 g/mol
Thermal Properties Metric English Comments
Flash Point 85.0 °C
185 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.445
1.445
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Adhesion to Vinyl/PVC-U yes
Appearance clear
Color light straw, yellow
Purity (%) 100