Dow Corning Z-6458 CHLOROSILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-6458 CHLOROSILANE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chlorosilane intermediate for siloxane manufactureInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc

@Temperature 25.0 °C
1.00 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 1.0 cSt
1.0 cSt
Molecular Weight 247.7 g/mol
247.7 g/mol
Thermal Properties Metric English Comments
Boiling Point 230 °C
446 °F
Flash Point 85.0 °C
185 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 97
Color light yellow, white