Dow DOWLEX™ 2025G Linear Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Dow Chemical
Trade Name DOWLEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DOWLEX™ 2025G Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow
Physical Properties Metric English Comments
Density 0.9265 g/cc
0.03347 lb/in³
ASTM D792
Thickness 19.0 microns
0.750 mil
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Antiblock Level 2500 ppm
2500 ppm
Slip Level 650 ppm
650 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 13.8 MPa
2000 psi
ASTM D882
Film Tensile Strength at Yield, TD 14.8 MPa
2150 psi
ASTM D882
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
Elmendorf Tear Strength TD 650 g
650 g
ASTM D1922
Elmendorf Tear Strength, MD 8.92 g/micron
227 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 34.1 g/micron
867 g/mil
ASTM D1922
Dart Drop Test 150 g
0.331 lb
ASTM D1709
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Film Tensile Strength at Break, TD 40.0 MPa
5800 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 122 °C
252 °F
Dow Method (DSC)
Vicat Softening Point 113 °C
235 °F
ASTM D1525