Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow DOWLEX™ IP-10 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Dow Chemical
Trade Name DOWLEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DOWLEX™ IP-10 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Next Generation DOWLEX® IP-10 resin is a high density polyethylene resin specifically designed for reusable case applications including, poultry, fast food, automotive, retail, fresh produce, beverage (soft drinks), food service and chemicals, including plastics. Excellent processability is achieved with Next Generation DOWLEX IP-10 resin due to its easy flow at low temperatures. This material complies with FDA regulation 21 CFR 177.1520 c 3.2 (a) for food contact applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
Melt Flow 9.0 g/10 min

@Load 2.16 kg
9.0 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.0 MPa
2610 psi
Tensile Strength, Yield 23.0 MPa
3340 psi
Elongation at Break 680 %
680 %
Modulus of Elasticity 0.717 GPa
104 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 1.08 GPa
157 ksi
Izod Impact Resistance 5.90 J/cm²
28.1 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 129 °C
264 °F