DOW DS6D21 is intended for use in cast film processes. It is particularly suited for applications requiring high clarity.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Temperature 230 °C
8.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3620 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 10 %
10 %
molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus 0.758 GPa
110 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 142 °C
288 °F
Dow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 81.1 °C
178 °F
unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648