Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow DS6D82 Polypropylene Resin

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DS6D82 Polypropylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW DS6D82 is intended for use as a heat seal coating on oriented polypropylene (OPP) film.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 7.0 g/10 min

@Temperature 230 °C
7.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2750 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 11 %
11 %
molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus 0.550 GPa
79.7 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
Dow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 67.8 °C
154 °F
unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648