Material Notes:
Description: Engage® 8100 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer applications. It provides good impact properties in blends with polypropylene (PP) and polyethylene (PE). Engage® 8100 also provides high filler loading capability and outstanding peroxide cure capability. When crosslinked by peroxide, silane, or irradiation, it gives exceptional heat aging, compression set, and weather resistance properties, and may be used to produce high performance electrical insulation. The product form is free-flowing pellets.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792
Mooney Viscosity 23

@Temperature 121 °C
23

@Temperature 250 °F
ML 1 + 4; ASTM D1646
Melt Index of Compound 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Hardness, Shore D 22
22
ASTM D2240
Tensile Strength, Ultimate 10.3 MPa
1490 psi
508 mm/min; ASTM D638
Tensile Strength, Yield 2.10 MPa
305 psi
508 mm/min; ASTM D638
Elongation at Break 820 %
820 %
508 mm/min; ASTM D638
2% Secant Modulus 0.0136 GPa
1.97 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 60.0 °C
140 °F
DSC, 10°C/min; DuPont Test
Vicat Softening Point 39.0 °C
102 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Descriptive Properties Value Comments
Comonomer Content 38 wt%
Dow Method (<sup>13</sup>C NMR/FTIR)