Material Notes:
Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in processing and makes Engage® 8130 highly effective as an impact modifier in polyolefins or as a component in injection molding applications. The product form is free-flowing pellets.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.864 g/cc
0.0312 lb/in³
ASTM D792
Mooney Viscosity 5.8

@Temperature 100 °C
5.8

@Temperature 212 °F
ML 1 + 4; ASTM D1646
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength, Ultimate 2.00 MPa
290 psi
508 mm/min; ASTM D638
Tensile Strength, Yield 1.90 MPa
276 psi
508 mm/min; ASTM D638
Elongation at Break 760 %
760 %
508 mm/min; ASTM D638
2% Secant Modulus 0.00690 GPa
1.00 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Descriptive Properties Value Comments
Comonomer Content 42 wt%
Dow Method (<sup>13</sup>C NMR/FTIR)