Dow H349-02 Polypropylene Homopolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade , Polypropylene, Film Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow H349-02 Polypropylene Homopolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is desired.Main CharacteristicsGood gauge controlHigh drawabilityGood opticsComplies with U.S. FDA 21 CFR 177.1520(c)1.1aDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.4 MPa
4700 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus, 1% Secant 1360 MPa
197000 psi
ASTM D790
Izod Impact, Notched 0.214 J/cm

@Temperature 0.000 °C
0.401 ft-lb/in

@Temperature 32.0 °F
ASTM D256A
0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
DSC; Dow Method
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
Unannealed; ASTM D648
Optical Properties Metric English Comments
Haze 46 %
46 %
1000 microns; ASTM D1003
Copyright © lookpolymers.com All Rights Reserved