Material Notes:
Complies withU.S. FDA 21 CFR 177.1520 (c) 1.1FDA-DMFUnderwriters Laboratories Inc.Europe EU-Directive 2002/72/ECLondon Metal Exchange - Part 6B Rules - PolypropyleneCanadian HPFB No ObjectionDOW H700-12 Polypropylene Resin is intended for use in injection molding processes and is particularly suited for rigid packaging. This product is UL listed.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 162 °C
324 °F
DSC; Dow Method
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
Unannealed; ASTM D648