Material Notes:
DOW HDPE 38152M resin is a medium molecular weight distribution copolymer designed to offer good impact strength and stress crack resistance with excellent toughness. This resin has excellent processability over a wide range of molding conditions. Typical applications are base cups and general purpose applications. This material complies with FDA regulation 21 CFR 177.1520 (c) 3.1 for food contact applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
Viscosity 38000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
38000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
80000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
80000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
180000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
180000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 38 g/10 min

@Load 2.16 kg
38 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.0 MPa
1600 psi
Tensile Strength, Yield 20.7 MPa
3000 psi
Elongation at Break 300 %
300 %
Modulus of Elasticity 0.627 GPa
90.9 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.952 GPa
138 ksi
Izod Impact Resistance 2.67 J/cm²
12.7 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 116 °C
241 °F