Dow HDPE 65053N High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow HDPE 65053N High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW HDPE 65053N resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and rigidity with high impact strength. This resin has excellent processability over a wide range of molding conditions. Typical uses are thin wall and dairy containers, promo drink cups, etc. This material complies with FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
Viscosity 32000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
32000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
46000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
46000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
54000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
54000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 65 g/10 min

@Load 2.16 kg
65 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 6.5.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.3 MPa
1490 psi
Tensile Strength, Yield 20.7 MPa
3000 psi
Elongation at Break 200 %
200 %
Modulus of Elasticity 0.669 GPa
97.0 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 1.01 GPa
146 ksi
Izod Impact Resistance 3.74 J/cm²
17.8 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 124 °C
255 °F