Dow INTEGRAL™ 899A Monolayer Adhesive Film

Category Polymer , Adhesive , Film , Thermoset
Manufacturer Dow Chemical
Trade Name INTEGRAL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INTEGRAL™ 899A Monolayer Adhesive Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INTEGRAL 899A Adhesive Film is a versatile heat-activated film that bonds to such substrates as: Polyethylene, Nylon, Polyester, Fiberglass, Glass, Polyurethane Foams/Sheet, Acrylic Adhesives, Wood, Paperboard, Cotton, Non-wovens, Aluminum, and Galvanized Steel.Information provided by Dow
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 320 %
320 %
ASTM D882
Film Elongation at Break, TD 490 %
490 %
ASTM D882
Secant Modulus, MD 0.138 GPa
20.0 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.131 GPa
19.0 ksi
2% Secant; ASTM D882
Elmendorf Tear Strength, MD 5.51 g/micron
140 g/mil
ASTM D882
Elmendorf Tear Strength, TD 7.87 g/micron
200 g/mil
ASTM D882
Film Tensile Strength at Break, MD 24.8 MPa
3600 psi
ASTM D882
Film Tensile Strength at Break, TD 22.8 MPa
3300 psi
ASTM D882