Material Notes:
INTEGRAL 936 High Heat Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, cardboard, fiberglass, non-wovens, and rigid urethanes.Information provided by Dow
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 400 %
400 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Secant Modulus, MD 0.103 GPa
14.9 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.165 GPa
23.9 ksi
2% Secant; ASTM D882
Elmendorf Tear Strength, MD 10.0 g/micron
255 g/mil
ASTM D882
Elmendorf Tear Strength, TD 21.7 g/micron
550 g/mil
ASTM D882
Film Tensile Strength at Break, MD 34.5 MPa
5000 psi
ASTM D882
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
ASTM D882
Users viewing this material also viewed the following: