Dow ISOBIND™ 1088 Isocyanate Binder

Category Polymer
Manufacturer Dow Chemical
Trade Name ISOBIND™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow ISOBIND™ 1088 Isocyanate Binder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISOBIND™ 1088 is a polymeric MDI used in composite wood products. Highly reactive with wood and agrifiber components and known to bond furnish that is dried to a wide range of moisture contents. ISOBIND™ binder imparts excellent bond durability and dimensional stability to commodity and specialty composite panels made of wood or agrifibers. Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
Viscosity 200 cP
200 cP
Chemical Properties Metric English Comments
Acid Value 50
50
ppm HCl
Descriptive Properties Value Comments
Isocyanate Equivalent Weight 134.6
NCO Content wt% 31.2