Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow LDPE 170A Low Density Polyethylene, Blown Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow LDPE 170A Low Density Polyethylene, Blown Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW LDPE 170A resin is used for shrink and heavy duty blown film applications where optical clarity is desired. It contains medium level of antiblock additives. It complies with U.S. FDA regulation 21 CFR c 2.1 for food contact applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 40 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
Thickness 40.0 microns
1.57 mil
Melt Flow 0.70 g/10 min

@Load 2.16 kg
0.70 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
Film Tensile Strength at Yield, TD 11.4 MPa
1650 psi
Film Elongation at Break, MD 325 %
325 %
Film Elongation at Break, TD 510 %
510 %
Coefficient of Friction 0.50
0.50
Elmendorf Tear Strength MD 390 g
390 g
Elmendorf Tear Strength TD 290 g
290 g
Elmendorf Tear Strength, MD 9.80 g/micron
249 g/mil
Elmendorf Tear Strength, TD 7.30 g/micron
185 g/mil
Dart Drop 2.80 g/micron
71.1 g/mil
Film Tensile Strength at Break, MD 23.4 MPa
3390 psi
Film Tensile Strength at Break, TD 17.9 MPa
2600 psi
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
Gloss 58 %
58 %
45°
Processing Properties Metric English Comments
Processing Temperature 216 °C
421 °F
Film extrusion temperature