Dow LDPE 4005M Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow LDPE 4005M Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
Melt Flow 5.5 g/10 min

@Load 2.16 kg
5.5 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.3 MPa
1490 psi
Tensile Strength, Yield 9.00 MPa
1310 psi
Elongation at Break 600 %
600 %
Modulus of Elasticity 0.172 GPa
24.9 ksi
Molded Sample 2% Secant Modulus
Izod Impact, Notched (ISO) 48.0 kJ/m²

@Temperature -50.0 °C
22.8 ft-lb/in²

@Temperature -58.0 °F
Tensile Impact Strength 275 kJ/m²
131 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F