Material Notes:
DOW LDPE 4012M resin is a broad molecular weight distribution homopolymer designed to provide good impact strength, excellent flexibility and high stress crack resistance for housewares, toys and general purpose applications. This general purpose molding resin demonstrates good processability over a wide range of molding conditions. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 2.1 for food contact applications. The regulation should be consulted for complete details.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
Melt Flow 12 g/10 min

@Load 2.16 kg
12 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.6 MPa
1540 psi
Tensile Strength, Yield 9.17 MPa
1330 psi
Elongation at Break 100 %
100 %
Modulus of Elasticity 0.153 GPa
22.2 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.237 GPa
34.4 ksi
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature -50.0 °C
12.8 ft-lb/in²

@Temperature -58.0 °F
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
Users viewing this material also viewed the following: