Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Latex LXC 8430NA Carboxylated Styrene-Butadiene Latex

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Dow Chemical
Trade Name Latex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Latex LXC 8430NA Carboxylated Styrene-Butadiene Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Latex LXC 8430NA for carpet is a firm-hand latex for residential and commercial carpet applications. Latex LXC 8430NA also has good rewet strength and can be used in formulations for print-base carpet (carpet that is back coated for dimensional stability and then dyed such as kitchen prints).Benefits: Firm handHigh binding strengthExcellent wet strengthHigh tuft bindSelf curingLow odorExcellent mechanical stabilityExcellent filler acceptanceInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 52 %
52 %
Particle Size 1.4 µm
1.4 µm
pH 7.85
7.85
Brookfield Viscosity 176 cP
176 cP
#2 @ 50 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -2.00 °C
28.4 °F
Descriptive Properties Value Comments
Minimum film formation temperature 53.6°F