Dow Latex LXC 8437NA Carboxylated Styrene-Butadiene Latex

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Dow Chemical
Trade Name Latex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Latex LXC 8437NA Carboxylated Styrene-Butadiene Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Latex LXC 8437NA is a versatile residential and commercial carpet latex with a medium hand. Latex LXC 8437NA offers good tuftbind and delamination properties and has exceptional filler acceptance characteristics. In most cases, this latex has good compatibility properties making it an ideal choice as a blending latex.Benefits: Medium handGood filler acceptanceGood compatibility with other latexesInformation provided by Styron
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Solids Content 52 %
52 %
Particle Size 1.4 µm
1.4 µm
pH 7.8
7.8
Brookfield Viscosity 210 cP
210 cP
#2 @ 50 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -11.0 °C
12.2 °F