Dow Nordel® IP 4640 Low Cost General Purpose Hose

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dow Chemical
Trade Name Nordel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Nordel® IP 4640 Low Cost General Purpose Hose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationNordel® IP 4640
Physical Properties Metric English Comments
Density 1.157 g/cc
0.04180 lb/in³
Mooney Viscosity 37

@Temperature 100 °C
37

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 7.20 MPa
1040 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 423 %
423 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00260 GPa
0.377 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.00520 GPa
0.754 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.00640 GPa
0.928 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 29.6 kN/m
169 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 64 %

@Temperature 125 °C
64 %

@Temperature 257 °F
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
Thermal Properties Metric English Comments
Brittleness Temperature -36.0 °C
-32.8 °F
Temperature Retraction, TR-10