FormulationNordel® IP 4725P
Physical Properties Metric English Comments
Density 1.168 g/cc
0.04220 lb/in³
Mooney Viscosity 31

@Temperature 100 °C
31

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 13.4 MPa
1940 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 360 %
360 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00550 GPa
0.798 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.0103 GPa
1.49 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.0128 GPa
1.86 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 48.5 kN/m
277 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 76 %

@Temperature 125 °C
76 %

@Temperature 257 °F
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
Thermal Properties Metric English Comments
Brittleness Temperature -21.0 °C
-5.80 °F
Temperature Retraction, TR-10