Material Notes:
Description: NDR 47100 is a developmental product in granular form that contains carbon black as a partitioning agent. It is a high molecular weight semi-crystalline EPDM grade with high green strength that is designed for applications requiring high compound green strength and good tensile properties. It can also be used as a blend component to enhance green strength. It offers fast cure rates and high states of cure with standard sulfur cure systems. This product is suited for applications such as industrial hoses, radiator hoses and extruded profiles.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D297
Volatiles <= 0.40 %
<= 0.40 %
Total Volatiles; DuPont Dow EPRG-21
Mooney Viscosity 100

@Temperature 125 °C
100

@Temperature 257 °F
Polymer (calculated), ML 1 + 4
Thermal Properties Metric English Comments
Crystallization Temperature 40.0 °C
104 °F
Onset; DuPont Test
Descriptive Properties Value Comments
Carbon Black Content (N650) 32 phr
DuPont Dow EPRG-2
ENB 4.9 mass%
ASTM D6047
Ethylene 73 mass%
ASTM D3900
Propylene TBD
ASTM D3900