Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow PELLETHANE® 2101-85A Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow PELLETHANE® 2101-85A Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PELLETHANE® 2101-85A offers good low temperature properties, fast cycle time, and good hydrolytic stability. Applications include: seals, gaskets, animal tags, molding applications, hose jacket.Data provided by Dow Chemical.Lubrizol acquired the Pellethane product line from Dow in 2009.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Melt Index of Compound 45 g/10 min

@Load 1.20 kg,
Temperature 224 °C
45 g/10 min

@Load 2.65 lb,
Temperature 435 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 84 - 92
84 - 92
ASTM D2240
Tensile Strength, Ultimate 28.0 MPa
4060 psi
ASTM D412
Elongation at Break 590 %
590 %
ASTM D412
100% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
300% Modulus 0.0129 GPa
1.87 ksi
ASTM D412
Tear Strength 111 kN/m
633 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 40
40
H-22 wheel (coarser); ASTM D1044
Compression Set 81 %

@Temperature 70.0 °C
81 %

@Temperature 158 °F
22 hrs.; ASTM D395, Method B
Tensile Set 120 %
120 %
Elongation Set After Break; ASTM D412
Thermal Properties Metric English Comments
Vicat Softening Point 109 °C
228 °F
ASTM D1525
Glass Transition Temp, Tg -24.0 °C
-11.2 °F
DSC
Processing Properties Metric English Comments
Melt Temperature 204 - 221 °C
399 - 430 °F
Users viewing this material also viewed the following: