Material Notes:
Data provided by Dow Chemical.
Physical Properties Metric English Comments
Melt Flow 5.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.9 MPa
2600 psi
ASTM Data
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM Data
Elongation at Break 30 %
30 %
ASTM Data
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM Data
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
Annealed; ASTM Data
Vicat Softening Point 101 °C
214 °F