Data provided by Dow Chemical.
Physical Properties Metric English Comments
Melt Flow 6.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM Data
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM Data
Elongation at Break 30 %
30 %
ASTM Data
Izod Impact, Notched 1.01 J/cm
1.89 ft-lb/in
ASTM Data
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.6 °C
168 °F
Annealed; ASTM Data
Vicat Softening Point 102 °C
216 °F