Dow SPECTRIM™ MM310 Reaction Moldable Polymer

Category Polymer , Thermoset
Manufacturer Dow Chemical
Trade Name SPECTRIM™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow SPECTRIM™ MM310 Reaction Moldable Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SPECTRIM™ MM 310 reaction moldable polymer is a three-component, fast-reacting, low viscosity polycarbamate system ideally suited for mat molding of structural composites. The structural reaction injection molding (SRIM) process uses conventional RIM equipment to produce structural composites by injection of a reaction moldable system onto a pre-placed fiber reinforcement.Information provided by Dow
Processing Properties Metric English Comments
Mold Temperature 54.4 - 65.6 °C
130 - 150 °F
45 secs De-mold Time
Injection Pressure 6.89 - 10.3 MPa
1000 - 1500 psi
Gel Time 0.167 - 0.200 min
0.167 - 0.200 min