Material Notes:
STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibration dampening component in packaging, material transport, and automotive applications.Information provided by Dow
Physical Properties Metric English Comments
Density 0.0400 g/cc
0.00145 lb/in³
DIN 53420
Mechanical Properties Metric English Comments
Compressive Strength 0.117 MPa
17.0 psi
at 25%, Horizontal; ASTM D3575, Suffix D
0.138 MPa
20.0 psi
at 25%, Vertical; ASTM D3575, Suffix D
0.317 MPa
46.0 psi
at 25%, Extruded; ASTM D3575, Suffix D
Compressive Modulus 0.00130 GPa
0.189 ksi
Horizontal; ASTM D3575, Suffix D
0.00174 GPa
0.252 ksi
Vertical; ASTM D3575, Suffix D
0.00965 GPa
1.40 ksi
Extruded; ASTM D3575, Suffix D
Heat Distortion <= 1.0 %
<= 1.0 %
linear change at 180°F; ASTM D3575, Suffix S
Thermal Properties Metric English Comments
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
Horizontal; ASTM D696
72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
Extrusion; ASTM D696
73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
Vertical; ASTM D696
Thermal Conductivity 0.0448 W/m-K
0.310 BTU-in/hr-ft²-°F
ASTM D3575, Suffix V