Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow STRANDFOAM™ EA 1600 Polypropylene Foam

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Foamed
Manufacturer Dow Chemical
Trade Name STRANDFOAM™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow STRANDFOAM™ EA 1600 Polypropylene Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
STRANDFOAM™ EA 1600 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibration dampening component in packaging, material transport, and automotive applications.Information provided by Dow
Physical Properties Metric English Comments
Density 0.0640 g/cc
0.00231 lb/in³
DIN 53420
Mechanical Properties Metric English Comments
Compressive Strength 0.290 MPa
42.0 psi
at 25%, Horizontal; ASTM D3575, Suffix D
0.331 MPa
48.0 psi
at 25%, Vertical; ASTM D3575, Suffix D
0.669 MPa
97.0 psi
at 25%, Extruded; ASTM D3575, Suffix D
Compressive Modulus 0.01362 GPa
1.975 ksi
Vertical; ASTM D3575, Suffix D
0.02237 GPa
3.245 ksi
Horizontal; ASTM D3575, Suffix D
0.02839 GPa
4.117 ksi
Extruded; ASTM D3575, Suffix D
Heat Distortion <= 1.0 %
<= 1.0 %
linear change at 180°F; ASTM D3575, Suffix S
Thermal Properties Metric English Comments
Thermal Conductivity 0.0390 W/m-K
0.270 BTU-in/hr-ft²-°F
ASTM D3575, Suffix V
Users viewing this material also viewed the following: