Material Notes:
FormulationTyrin® CPE Elastomer
Physical Properties Metric English Comments
Mooney Viscosity >= 37

@Temperature 121 °C
>= 37

@Temperature 250 °F
ML 1 + 4; ASTM D1646
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength, Ultimate 17.9 MPa
2600 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
200% Modulus 0.00970 GPa
1.41 ksi
ASTM D412