Dow VORANATE™ T-80 toluene diisocyanate (TDI)

Category Polymer
Manufacturer Dow Chemical
Trade Name VORANATE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow VORANATE™ T-80 toluene diisocyanate (TDI).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VORANATE™ T-80 TDI products are designed for a variety of high-resilience molding, TDI molding, formulating (systems) and flexible slabstock applications. They are used in the production of flexible polyurethane foams for furniture, bedding, and automotive seating and padding. In addition, VORANATE™ T-80 TDI products are used in the production of elastomers, coatings, adhesives, semi-flexible foams, and carpet underlayment and backing.Information provided by Dow
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Viscosity Measure 2.5 cSt

@Temperature 25.0 °C
2.5 cSt

@Temperature 77.0 °F
Molecular Weight 174.2 g/mol
174.2 g/mol
Vapor Pressure 0.0000133 bar
0.0100 torr
Thermal Properties Metric English Comments
Specific Heat Capacity 1.46 J/g-°C

@Temperature 20.0 °C
0.349 BTU/lb-°F

@Temperature 68.0 °F
1.72 J/g-°C

@Temperature 100 °C
0.411 BTU/lb-°F

@Temperature 212 °F
Melting Point 14.0 °C
57.2 °F
Boiling Point 120 °C
248 °F
10 mm Hg
250 °C
482 °F
760 mm Hg
Decomposition Temperature 287 °C
549 °F
Flash Point 126 °C
259 °F
Pensky Martens closed cup
Optical Properties Metric English Comments
Refractive Index 1.5662
1.5662